(Summary description)How to control the quality of the longitudinally welded pipe? The perforation temperature of the blank varies depending on the raw material. Thermal expansion welded pipes are mostly around 1200°C, and the temperature is slightly lower when the carbon content and other alloying elements are high.

Quality Control Requirements for Longitudinal Welded Pipes

(Summary description)How to control the quality of the longitudinally welded pipe? The perforation temperature of the blank varies depending on the raw material. Thermal expansion welded pipes are mostly around 1200°C, and the temperature is slightly lower when the carbon content and other alloying elements are high.

Information
How to control the quality of the longitudinally welded pipe? The perforation temperature of the blank varies depending on the raw material. Thermal expansion welded pipes are mostly around 1200°C, and the temperature is slightly lower when the carbon content and other alloying elements are high.
 
       The second key to heating operation is to minimize the amount of oxide scale. Especially in the heat kneading elbow, the heat expansion welded pipe starts from the east-west life and the surface quality of the kneaded pipe, and the request becomes more severe.
 
       In the production process of longitudinally welded pipes, since the primary processing is carried out in a hot state, the heating operation is a very important process for determining the quality of the product.
 
       Heating furnaces are divided into heating furnaces and reheating furnaces according to their effects; the former is used to heat the billet from room temperature to the processing temperature; the latter is used to reheat the billet to the necessary processing during processing temperature.
 
       Improper heating will be the cause of waste products such as cracks, folds, and pain on the inner or outer surface of the tube blank.
 
       There are many types of hot blast stoves, but the first to use is the ring heating stove. This kind of heating furnace has a ring-shaped furnace bottom, which can be slowly transformed. The billet is loaded from the entrance along the diameter of the furnace bottom, and it can be heated and soaked to a regular temperature as soon as it is used at the exit. A kind of stove. The key to this heating operation is to uniformly heat the billet to a temperature suitable for processing. Since perforation has a great influence on quality, that is to say, the temperature during the bending process is an important condition that affects the quality, so it is generally necessary to control the temperature of the blank during the perforation process.

Scan the QR code to read on your phone

09-10

2021

What should be paid attention to in the maintenance of stainless steel elbow

There are many problems in the use and maintenance of stainless steel elbows, which require users to use them in a certain way, and use and maintain them in an accurate and fair manner. The considerations are as follows:   1. Stainless steel elbows stored for a long time should be checked in time, and the exposed surface should be kept clean, dirt removed, and stored neatly in a ventilated and dry place indoors. Stacking or open storage is strictly prohibited. Stainless steel elbows are always kept dry and breathable, and the holder is clean and tidy, and stored in accordance with accurate storage methods.   2. During installation, the stainless steel elbow can be directly installed on the pipeline according to the connection method, and the stainless steel elbow can be installed according to the location of use. Under normal circumstances, it can be installed in any position of the pipeline, but it requires easy-to-operate inspection. Note that the flow of the stainless steel elbow medium should flow under the longitudinal valve flap, and the stainless steel elbow can only be installed horizontally. When installing the stainless steel elbow, pay attention to sealing to prevent leakage and affect the normal operation of the pipeline. 3. When using stainless steel elbow ball valves, globe valves and gate valves, they can only be opened or closed, and the flow rate must not be adjusted to avoid wear of the sealing surface. The gate valve and the upper threaded globe valve are equipped with an inverted sealing device, and the handwheel is fastened to the top to prevent media Leakage from the filling point.    4. Use the hand wheel to make stainless steel elbows. Do not use levers or other tools to avoid damage to valve components. Turn the handwheel clockwise to close, and vice versa. When using, we should be fair and ensure the correct use of methods and means.   5. The bolts of the stainless steel elbow valve packing cover should be evenly tightened, and should not be pressed into a bent state, so as not to interfere with the movement of the valve stem or cause leakage.    6. The stainless steel elbow should be kept clean during use, and the transmission thread must be lubricated in time. Once a fault is found, it should be stopped immediately to find out the cause of the fault.

Service
Service hotline
086 316-7515381 086 316-7515381
Service time:
8:00 - 24:00
Service:
Online service
WhatsApp:

Hotline:

086 316-7515381

Address:Dongjiabao Village, Dongduan Township, Bazhou City, Hebei Province , China.
Tel:
086 316-7515381 7515382  7515887

WeChart

erweima

Message 

Username used for comment:
客户留言
Description:
验证码

Copyright © 2021 Hebei Shengbao Pipe Manufacturing Co., Ltd.   Powered by www.300.cn   冀ICP备2021017406号

Copyright © 2021 Hebei Shengbao Pipe Manufacturing Co., Ltd.

Powered by www.300.cn   冀ICP备2021017406号